Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N3HG6 LS BK - PA9T-GF30 - BASF

Material Data Center offers the following functions for Ultramid® Advanced N3HG6 LS BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
部分芳香族玻璃纤维增强聚邻苯二甲酰胺,可用于注塑成型。具有很强的机械性能,尤其是在高温下,具有良好的长期热稳定性和对高应力零件的出色耐化学性。该产品的特点是具有高韧性、刚度、极低的吸水率和出色的尺寸稳定性。它具有高流动性,可以填充壁厚较薄的复杂零件。该产品易于加工,具有出色的熔体稳定性。

市场与应用
汽车:燃油系统,冷却系统,进气系统(EGR),汽车电子电气,传感器,泵,燃料电池
E&E:连接器
消费品:家用电器,消费类电子产品
加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 0.5 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.9 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 10000 / 10000 MPa ISO 527
断裂应力 185 / 160 MPa ISO 527
断裂伸长率 2.4 / 2 % ISO 527
无缺口简支梁冲击强度, +23°C 60 / 40 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 60 / 60 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 8 / 6 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 8 / - kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 300 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 120 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 270 / * °C ISO 75-1/-2
维卡软化温度, B 280 / * °C ISO 306
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 1MHz 3.6 / 3.6 - IEC 62631-2-1
介质损耗因子, 1MHz 125 / 190 E-4 IEC 62631-2-1
表面电阻率 * / >1E15 Ohm IEC 62631-3-2
相对漏电起痕指数 - / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 2 / * % 类似ISO 62
吸湿性 0.9 / * % 类似ISO 62
密度 1370 / - kg/m³ ISO 1183
模塑测量的特殊性能干 / 已调节单位Test Standard
ISO数据
粘数 100 / * cm³/g ISO 307, 1157, 1628
加工推荐(注塑)价值单位Test Standard
预干燥-温度 120 °C -
预干燥-时间 8 h -
加工湿度 ≤0.05 % -
注塑熔体温度 320 - 340 °C -
模具温度 100 - 160 °C -
函数
应力-应变.  , Ultramid® Advanced N3HG6 LS BK (烘干), PA9T-GF30, BASF
应力-应变.  , Ultramid® Advanced N3HG6 LS BK (状况), PA9T-GF30, BASF
正割模量-应变.  , Ultramid® Advanced N3HG6 LS BK (烘干), PA9T-GF30, BASF
正割模量-应变.  , Ultramid® Advanced N3HG6 LS BK (状况), PA9T-GF30, BASF
应力-应变(等时的) 23°C, Ultramid® Advanced N3HG6 LS BK (状况), PA9T-GF30, BASF
蠕变模量-时间. 23°C, Ultramid® Advanced N3HG6 LS BK (状况), PA9T-GF30, BASF
蠕变曲线 23°C, Ultramid® Advanced N3HG6 LS BK (状况), PA9T-GF30, BASF
拉伸模量-温度 , Ultramid® Advanced N3HG6 LS BK (烘干), PA9T-GF30, BASF
拉伸模量-温度 , Ultramid® Advanced N3HG6 LS BK (状况), PA9T-GF30, BASF
典型数据
加工方法
注塑
供货形式
粒料, 黑色
特殊性能
经热稳处理的/耐热的
特征
熔体强度, 热稳定性
耐化学试剂
通用耐化学性
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 320 - 340 °C
injection molding, Melt temperature, recommended: 330 °C
injection molding, Mold temperature, range: 125 - 170 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 5 min
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.